whats the best method for rubbing down paint between coats..... When spraying (airbrush) my tr4, i primed and rubbed down with a 3000 grit (wet and dry), then applyed a colour coat and repeated rub down, dont know if i was being a bit heavy handed but seemed to be taking of to much paint, although i thought i was very careful, applied another coat and repeated, same again, but obviously started losing panel line definition.... So started losing heart, went and ate chocolate.... Put to the back of the shelf and started beetle, have now applied first colour coat to this model, and would like advice on how to proceed, would really like to get this right