Scale Model Shop

Collapse

Sorry me again, advice on 2 part epoxy putty

Collapse
X
 
  • Time
  • Show
Clear All
new posts
  • BattleshipBob
    SMF Supporters
    • Apr 2018
    • 6803
    • Bob
    • Cardiff

    #1

    Sorry me again, advice on 2 part epoxy putty

    Evening all

    Will need to use 2 part epoxy putty ( right name???? )

    Any advice on how to use and best too buy. Hopefully one which does not cure too quick. Sorry to be a pain

    Will need it on the Hood build

    Ta bob
  • Airborne01
    • Mar 2021
    • 3996
    • Steve
    • Essex

    #2
    Dependent on usage and cost - Milliput? Works for me in many ways ...
    Steve

    Comment

    • stillp
      SMF Supporters
      • Nov 2016
      • 8096
      • Pete
      • Rugby

      #3
      What will you use it for? Milliput is good, but car body filler is cheaper.
      Pete

      Comment

      • stona
        • Jul 2008
        • 9889

        #4
        For what it's worth, when I resort to epoxy I use the clear 15 minute Araldite, but that may be too quick for you, depending what you are doing with it.

        I sometimes apply it as it starts to 'go off' because it is less viscous and more likely to stay where I want it (rather than on odd parts of the model, my shirt, the neighbour's cat, etc.) :smiling3:

        For a filler I occasionally use Milliput (fine).

        Comment

        • BattleshipBob
          SMF Supporters
          • Apr 2018
          • 6803
          • Bob
          • Cardiff

          #5
          Sorry should have said

          To partially fill the bow of Hood, then hopefully drill through it connecting the hawse pipes for the anchor chain to run from the capstans to the anchors

          Comment

          • stillp
            SMF Supporters
            • Nov 2016
            • 8096
            • Pete
            • Rugby

            #6
            Seems like a job for car body filler to me. Whatever you use, check if a big lump of it heats up when curing, if it does there's a risk of distorting the plastic. Maybe Milliput would be safer, I don't think that gets hot but I could be wrong.
            Pete

            Comment

            • Tim Marlow
              SMF Supporters
              • Apr 2018
              • 18925
              • Tim
              • Somerset UK

              #7
              I’d go with milliput Bob. Doesn’t heat up on reaction and can be smoothed with damp tools to minimise clean up.

              Comment

              • Tworrs
                SMF Supporters
                • Jan 2022
                • 1982
                • Garry
                • New Zealand

                #8
                I would use Milliput for that Bob.
                Strength isn't about what you can do, rather it's about overcoming what you thought you couldn't do.

                Comment

                • Ian M
                  Administrator
                  • Dec 2008
                  • 18271
                  • Ian
                  • Falster, Denmark

                  #9
                  Milliput as already said.
                  Sets hard and can be drilled (you can even tap a thread in it!). Can be cleaned and smoothed with wet tools/finger/cotton bud etc.
                  There are several different ones. I normally go with the white one.
                  Group builds

                  Bismarck

                  Comment

                  • Neil Merryweather
                    SMF Supporters
                    • Dec 2018
                    • 5197
                    • London

                    #10
                    Originally posted by Ian M
                    Milliput as already said.
                    Sets hard and can be drilled (you can even tap a thread in it!). Can be cleaned and smoothed with wet tools/finger/cotton bud etc.
                    There are several different ones. I normally go with the white one.
                    With respect Ian, if you've not used Milliput before I would recommend the regular one, it's easier to get the mix right with the different coloured components. And it's cheaper.
                    That said, if it needs sanding back after curing , Milliput is MUCH harder than car body filler and could result in accidental damage to the plastic. BUT I do take the point about the heat reaction with car body filler.
                    Just reading Bob's description again though,sounds like the fill will be totally inside the model so milliput is probably the safest,it will give you about 90 mins working time Bob, and you could even start the hole while it's still workable.
                    Good luck Bob

                    Comment

                    • Scratchbuilder
                      • Jul 2022
                      • 2689

                      #11
                      Probably too late Bob, but I use car Stopping filler. It is available from car outlets like Halfords, comes in a tube and lasts for ages.

                      Comment

                      • boatman
                        SMF Supporters
                        • Nov 2018
                        • 14498
                        • christopher
                        • NORFOLK UK

                        #12
                        WELL Boyo i use plastic wood filler on my tiger an it comes in a tin or a tube an very good but a bit exspensive about 4 quid for a tube but it will sand down to a nice finish
                        chrisb

                        Comment

                        • rtfoe
                          SMF Supporters
                          • Apr 2018
                          • 9092

                          #13
                          Well Bob, fillers usually shrink and if it's where you mentioned it's better with two part putty like Milliput or Magic Sculpt. These have a work time of about half an hour to 90 mins. doesn't shrink and is paintable while curing.

                          Cheers,
                          Wabble

                          Comment

                          • Guest

                            #14
                            Contrary to all the other advice above, I will say: Stay away from Milliput — it’s bloody awful crap that’s hard to mix and goes off (when unused) within a few years so it gets even harder to mix. About the only reasonably usable kind they have is the “superfine white” variety, but that has the problem that you’ll be mixing one part white to one part off-white, making it very difficult to tell if you’ve mixed them enough or will end up with eternal chewing gum.

                            Almost every other brand of two-part epoxy putty aimed at modellers, is better, in my experience. I have a packet of Sylmasta A+B that’s over twenty years old and still works perfectly, as well as Magic Sculp that’s maybe five years younger and is still fine too. Both have the great advantage of being much softer than Milliput, making them much easier to mix.

                            Comment

                            • Neil Merryweather
                              SMF Supporters
                              • Dec 2018
                              • 5197
                              • London

                              #15
                              Magic Sculp is definitely more forgiving than Milliput, I'd forgotten about that

                              Comment

                              Working...